      • SEPLITE® Monojet™ SA8500CP (historical reference SA550CP) Ion Exchange Resin is a high-quality, high-capacity resin with uniform particle size designed specifically for use in condensate polishing mixed beds when high purity and water quality are required.With its smaller average particle size which provides excellent beads integrity and good kinetics, it is suitable for the high flow rate demands of condensate polishing applications. This resin could be available in both OH- form and Cl- form, the ionic conversion rate of OH- form is up to 95%.The resin is normally paired with SEPLITE® Monojet™ SC7700CP (SC650CP) in H+ form in mixed beds, providing excellent water quality and resin purity.

        Please contact us at for specific academic pricing.

    • Properties
      • Categories
        Gel Type, Strong Base, ST-DVB, OH- Form, High Capacity, Uniform Particle Size
        Other Properties
        Matrix Structure: Gel, Styrene-divinylbenzene
        Functional group: Trimethylammonium
        Shipping form: OH-
        Physical Appearance: White to yellow translucent spherical beads
        Particle size (mm): 0.59±0.05mm
        Moisture content (%): 55-65 (OH- Form)
        Total Capacity(eq/L): ≥1.0 (OH- Form)
        Bulk Density ( g/l): 660-720
        Density ( g/l): 1080-1100
        Whole beads count (%): ≥95
        Uniformity coefficient: ≤1.2
        Note
        Resins should be stored in sealed containers or bags where temperature was above 0°C in dry conditions without exposure to direct sunlight.
        Do not mix ion exchange resin with strong oxidizing agents; otherwise it will cause violent reactions.
        In case of eyes contact with resins, rinse eyes immediately with plenty of water, and consult a specialist.
        Material and samples must be disposed according to local regulations.
        Dry polymers will expand when become wetted and may cause an exothermic reaction.
        Spilled materials may be slippery.
    • Applications
      • Application
        Condensate Polishing

Note: If you don't receive our verification email, do the following:

  • Confirm that you entered your email address correctly.
  • Check if the email is in your spam or junk folder.
  • Or you may contact us at .
  • Copyright © Amerigo Scientific. All rights reserved.