SEPLITE® Monojet™ SA6400F Strong Base Anion Exchange Resin

SEPLITE® Monojet™ SA6400F Strong Base Anion Exchange Resin

Catalog Number:
SBAE110771SUN
Mfr. No.:
SA6400F
Price:
Quantity:
Add to Cart:
    • Overview
      • SEPLITE® Monojet™ SA6400F Ion Exchange Resin is a sugar grade gel type 1, strong basic anion resin with beads of uniformsize (monojetted).The structure is specially developed to make a balance between total capacity and regeneration efficiency. It also has excellent resistance to osmotic shock and good physical and chemical stability.With its stable chemical and physical properties, the resin is able to yield excellent operation capacity but with low pressure drop, which can aso help the users to save the usage of regenerant and rinse water.SEPLITE® Monojet™ SA6400F is also available in OH-form depending on user’s requirement.

        Please contact us at for specific academic pricing.

    • Properties
      • Categories
        Gel Type I, Strong Base, ST-DVB, Cl- Form, Uniform Particle Size
        Other Properties
        Matrix Structure: Gel, Styrene-divinylbenzene
        Functional group: Trimethylammonium
        Shipping form: Cl- (OH- is also available)
        Physical Appearance: Light yellow to yellowish translucent spherical beads
        Particle size (mm): 0.65±0.05mm
        Moisture content (%): 49-55 (Cl- Form)
        Total Capacity(eq/L): ≥1.2 (Cl- Form)
        Bulk Density ( g/l): 660-750
        Density ( g/l): 1060-1100
        Whole beads count (%): ≥95
        Uniformity coefficient: ≤1.1
        Volume change (Cl- to OH-) Max. vol.%: 20
        Note
        Resins should be stored in sealed containers or bags where temperature was above 0°C in dry conditions without exposure to direct sunlight.
        Do not mix ion exchange resin with strong oxidizing agents; otherwise it will cause violent reactions.
        In case of eyes contact with resins, rinse eyes immediately with plenty of water, and consult a specialist.
        Material and samples must be disposed according to local regulations.
        Dry polymers will expand when become wetted and may cause an exothermic reaction.
        Spilled materials may be slippery.
    • Applications
      • Application
        Industrial Demineralization

Note: If you don't receive our verification email, do the following:

  • Confirm that you entered your email address correctly.
  • Check if the email is in your spam or junk folder.
  • Or you may contact us at .
  • Copyright © Amerigo Scientific. All rights reserved.