SEPLITE® Monojet™ LSC7500 Chelating Resin

SEPLITE® Monojet™ LSC7500 Chelating Resin

Catalog Number:
CR03110708SUN
Mfr. No.:
LSC7500
Price:
Quantity:
Add to Cart:
    • Overview
      • SEPLITE® Monojet™ LSC7500 is a weak acid, macroporous, chelating resin with amino phosphonic acid groups. This structure is good for the chelating with heavy metal ions.
        Compared with the chelating resin with amino carboxylic acid groups, resins with amino phosphonic acid groups are much easier to chelating with certain cation ions. SEPLITE® Monojet™ LSC7500(amino phosphonic acid) is more suitable for purification the second brine during production of membrane caustic soda.
        For SEPLITE® Monojet LSC7500(amino phosphonic acid), it enjoys the advantage of below:
        1)Superior mechanical and excellent resistance to osmotic shock:
        Good mechanical strength, low loss, less topping annually, stable Kinetics performance
        2)High chelating capacity:
        High chelating capacity leads to bigger amount of brine treated per cycle
        3)More uniform for particle size:
        Excellent running kinetics during regeneration

        Please contact us at for specific academic pricing.

    • Properties
      • Categories
        Weak acid, macroporous, chelating resin with amino phosphonic acid groups
        Other Properties
        Matrix Structure: Polystyrene DVB, Macroporous
        Functional group: Amino phosphonic acid
        Shipping form: Na+
        Physical Appearance: Gray to light yellow spheres
        Particle range (mm): 0.55-0.65 (≥95%)
        Moisture Content (%): 55-65
        Bulk Density (g/l): 700-800
        Density (g/l): 1150-1250
        Total capacity (eq/L): ≥2.5
        Uniformity coefficient: ≦1.1
        Volume change Na-H (Max.): -30%
        Note
        Resins should be stored in sealed containers or bags where temperature was above 0 °C in dry conditions without exposure to direct sunlight. Do not mix ion exchange resin with strong oxidizing agents; otherwise it will cause violent reactions.
        In case of eyes contact with resins, rinse eyes immediately with plenty of water, and consult a specialist. Material and samples must be disposed according to local regulations.
        Dry polymers will expand when become wetted and may cause an exothermic reaction. Spilled materials may be slippery.
    • Applications
      • Application
        Brine Purification

Note: If you don't receive our verification email, do the following:

  • Confirm that you entered your email address correctly.
  • Check if the email is in your spam or junk folder.
  • Or you may contact us at .
  • Copyright © Amerigo Scientific. All rights reserved.